How Is SBS Processed? Common Processing Methods and Key Considerations
Nov 26, 2026
Styrene Butadiene Styrene (SBS) is a versatile thermoplastic elastomer (TPE) that bridges the gap between vulcanized rubber elasticity and thermoplastic melt-processability. Its block copolymer structure consists of polystyrene (PS) hard segments and polybutadiene (PB) soft segments. The polystyrene end blocks form physical crosslinks through microphase separation, while the polybutadiene midblock provides flexibility and elastic recovery.
1. Common SBS Processing Methods
SBS Injection Molding
Injection molding is the primary route for high-volume, dimensionally accurate parts such as footwear outsoles, soft-touch grips, gaskets, and shock-absorbing pads. SBS grades with suitable melt flow characteristics (such as Sinopec SBS YH-805E) are generally preferred for efficient cavity filling and consistent molding quality.
Barrel Temperature Profile: 170°C–190°C
Injection Pressure: 60–100 MPa
Mold Cooling Time: 20–40 seconds (depending on wall thickness)
Key Trade-Off: Offers high production efficiency and good dimensional consistency, although mold fabrication costs may make it less economical for oversized components or small production runs.
SBS Extrusion Processing
Extrusion converts SBS (such as Sinopec SBS YH-791E) compounds into continuous cross-sections, including automotive sealing strips, flexible hoses, sheets, and wire/cable insulation.
Screw Geometry: An L/D ratio of approximately 18:1 and a compression ratio of 2.5:1 can serve as reference parameters for the specified extrusion configuration. Screw design should be matched to the SBS grade and processing requirements to ensure consistent melting and stable material flow.
Temperature Zones: Feed zone at 150°C → Metering zone at 180°C → Die head at 190°C.
Haul-Off Synchronization: Puller speed must be synchronized with the extrusion output to maintain dimensional consistency and minimize necking, deformation, and residual stress in the finished products.
SBS Calendering
Calendering is ideal for wide-web flexible sheets, waterproofing membranes, and specialty packaging films where uniform gauge control is critical.
Typical Calendering Process: Internal compounding → Pre-heating (160°C) → Four-roll calendering (roll temperature maintained at 170°C) → Controlled cooling and wind-up.
Advanced Film Capability: Calendering can be used to produce flexible SBS sheets and films with thicknesses of approximately 0.1–0.5 mm, depending on the formulation and processing conditions. Final film clarity and thickness uniformity are influenced by material properties, roll conditions, and cooling parameters.
2. Comparison of Different SBS Processing Methods
Processing method
Typical products
Production Efficiency
Tooling & Equipment Cost
Injection Molding
Shoe soles, grips, molded components
High
High
Extrusion
Profiles, strips, sheets
Medium
Medium
Calendering
Sheets and films
Low
Low
The choice of processing method should depend on the final product requirements rather than production equipment alone. Injection molding is more suitable for shaped components, while extrusion is generally preferred for continuous profiles. Calendering is an option for applications requiring controlled sheet thickness.
3. Advanced Processing Technologies for SBS Materials
Microcellular Injection Molding
Introducing supercritical CO₂ into the SBS melt can generate a microcellular structure during molding. For suitable SBS formulations, this process may reduce finished part weight by 15%–20%, depending on the foaming conditions and material formulation. The resulting cellular structure can also influence cushioning, mechanical properties, and thermal insulation performance, making the technology worth exploring for footwear components and automotive interior applications.
3D Printing with SBS-Based Materials
Specially formulated SBS based filaments may be used for the rapid prototyping of flexible components, such as custom gaskets and wearable parts. For the tested SBS based filament, a nozzle temperature of 185°C ± 5°C and a layer height of 0.1–0.2 mm can serve as reference printing parameters. Actual settings should be adjusted according to filament composition, printer configuration, and printing speed.
Website: www.elephchem.com
whatsapp: (+)86 13851435272
E-mail: admin@elephchem.com
Read More